Inorganic Chemistry

Metallurgy: Isolation of Metals

From ore to pure metal, covering ores and concentration (froth flotation, magnetic separation, leaching), calcination and roasting, the thermodynamics of reduction and the Ellingham diagram, extraction of iron, copper, zinc and aluminium, and refining by distillation, liquation, electrolysis, zone refining and vapour phase methods

NEET style

Removed from the rationalised NCERT books and from the NEET UG syllabus since 2024, so expect at most a stray fact inside another chapter’s question

JEE style

Not in the JEE Main syllabus since 2024, while JEE Advanced still tests Ellingham diagram reading, roles of reagents (cryolite, NaCN depressant, silica flux, Zn in the cyanide process), refining methods and Faraday law numericals

Ores and concentration

Naturally occurring compounds of metals are minerals; a mineral from which a metal can be extracted profitably is an ore. The unwanted earthy material is gangue.

MetalImportant ores
AluminiumBauxite AlOXx(OH)X3−2x\ce{AlO_{x}(OH)_{3-2x}} (0 < x < 1); kaolinite [AlX2(OH)X4SiX2OX5]\ce{[Al2(OH)4Si2O5]}
IronHaematite FeX2OX3\ce{Fe2O3}, magnetite FeX3OX4\ce{Fe3O4}, siderite FeCOX3\ce{FeCO3}, iron pyrites FeSX2\ce{FeS2}
CopperCopper pyrites CuFeSX2\ce{CuFeS2}, malachite CuCOX3 ⋅ Cu(OH)X2\ce{CuCO3*Cu(OH)2}, cuprite CuX2O\ce{Cu2O}, copper glance CuX2S\ce{Cu2S}
ZincZinc blende (sphalerite) ZnS, calamine ZnCOX3\ce{ZnCO3}, zincite ZnO
  • Hydraulic washing (gravity separation): heavier ore particles settle in a stream of water.
  • Magnetic separation: magnetic ores (magnetite, wolframite) are separated from nonmagnetic gangue.
  • Froth flotation for sulfide ores: the ore is wetted by oil and carried up in the froth; the gangue is wetted by water and sinks. Collectors (pine oils, fatty acids, xanthates) make the mineral particles less wettable by water; stabilisers (cresols, aniline) stabilise the froth; a depressant such as NaCN keeps ZnS down while PbS floats.
  • Leaching dissolves the ore in a suitable reagent, as in the Bayer process for bauxite and the cyanide process for silver and gold.
  1. 1
    Bayer process: digest the powdered ore with concentrated NaOH at 473 to 523 K and 35 to 36 bar: AlX2OX3+2 NaOH+3 HX2O→2 Na[Al(OH)X4]\ce{Al2O3 + 2NaOH + 3H2O -> 2Na[Al(OH)4]} (silica dissolves as silicate; iron oxide and TiOX2\ce{TiO2} are left behind).
  2. 2
    Neutralise with COX2\ce{CO2}: 2 Na[Al(OH)X4]+COX2→AlX2OX3 ⋅ x HX2O↓+2 NaHCOX3\ce{2Na[Al(OH)4] + CO2 -> Al2O3*xH2O v + 2NaHCO3} (seeded with fresh hydrated alumina).
  3. 3
    Heat at 1470 K: AlX2OX3 ⋅ x HX2O→AlX2OX3+x HX2O\ce{Al2O3*xH2O -> Al2O3 + xH2O}.
4 M+8 CNX−+2 HX2O+OX2→4 [M(CN)X2]X−+4 OHX−\ce{4M + 8CN- + 2H2O + O2 -> 4[M(CN)2]- + 4OH-}

Cyanide leaching (M = Ag, Au); the metal is then displaced by zinc: 2[M(CN)₂]⁻ + Zn → [Zn(CN)₄]²⁻ + 2M

Calcination, roasting and the thermodynamics of reduction

Calcination

  • Heating in limited air or no air
  • For carbonates and hydrated oxides
  • ZnCOX3→ZnO+COX2\ce{ZnCO3 -> ZnO + CO2}
  • FeX2OX3 ⋅ x HX2O→FeX2OX3+x HX2O\ce{Fe2O3*xH2O -> Fe2O3 + xH2O}
  • Volatile matter (CO₂, H₂O) escapes

Roasting

  • Heating in a regular supply of air below the melting point
  • For sulfide ores
  • 2 ZnS+3 OX2→2 ZnO+2 SOX2\ce{2ZnS + 3O2 -> 2ZnO + 2SO2}
  • 2 PbS+3 OX2→2 PbO+2 SOX2\ce{2PbS + 3O2 -> 2PbO + 2SO2}
  • SO₂ is used to make sulfuric acid
Gibbs energy
ΔG∘=ΔH∘−TΔS∘=−RTln⁡K\Delta G^\circ = \Delta H^\circ - T\Delta S^\circ = -RT\ln K

Reduction of an oxide MXxO\ce{M_{x}O} by a reductant is feasible when the coupled reaction has ΔG∘<0\Delta G^\circ < 0, that is, when the oxidation of the reductant has a more negative ΔG∘\Delta G^\circ than the oxidation of the metal.

  • The Ellingham diagram plots ΔfG∘\Delta_fG^\circ against T for the formation of oxides per mole of OX2\ce{O2}.
  • Most lines slope upward: gaseous OX2\ce{O2} is consumed, so ΔS<0\Delta S < 0. The line for 2 C+OX2→2 CO\ce{2C + O2 -> 2CO} slopes downward (ΔS>0\Delta S > 0: one mole of gas becomes two), and C+OX2→COX2\ce{C + O2 -> CO2} is almost flat.
  • A metal (or C, CO) can reduce the oxide of any element whose line lies above it at that temperature. Where two lines cross, the reduction becomes feasible on one side of that temperature.
  • Above about 1073 K the C→CO line falls below the Fe→FeO line, so coke reduces FeO in the hotter part of the blast furnace (NCERT). The CO→CO₂ and C→CO lines cross near 983 K (a figure from outside NCERT): below this CO is the better reductant (NCERT’s answer at 673 K is CO), above it carbon is.
  • Limitation: the diagram shows only thermodynamic feasibility, not the rate of reduction.

Extraction of iron, copper, zinc and aluminium

Pig iron (about 4% C) is remelted to cast iron (about 3% C, hard and brittle), and wrought iron, the purest commercial iron, is made by oxidising the carbon in a furnace lined with haematite
Blast furnace zoneReactions
500 to 800 K (upper, cooler part)3 FeX2OX3+CO→2 FeX3OX4+COX2\ce{3Fe2O3 + CO -> 2Fe3O4 + CO2}; FeX3OX4+4 CO→3 Fe+4 COX2\ce{Fe3O4 + 4CO -> 3Fe + 4CO2}; FeX2OX3+CO→2 FeO+COX2\ce{Fe2O3 + CO -> 2FeO + CO2}
900 to 1500 K (lower, hotter part)C+COX2→2 CO\ce{C + CO2 -> 2CO}; FeO+CO→Fe+COX2\ce{FeO + CO -> Fe + CO2}
Slag formationCaCOX3→CaO+COX2\ce{CaCO3 -> CaO + CO2}; CaO+SiOX2→CaSiOX3\ce{CaO + SiO2 -> CaSiO3}
  1. 1
    Copper: roast the sulfide ore, then smelt with silica; iron oxide forms slag (FeO+SiOX2→FeSiOX3\ce{FeO + SiO2 -> FeSiO3}), leaving matte (CuX2S\ce{Cu2S} + FeS).
  2. 2
    In the silica lined converter, a hot air blast first removes the remaining iron as slag, then 2 CuX2S+3 OX2→2 CuX2O+2 SOX2\ce{2Cu2S + 3O2 -> 2Cu2O + 2SO2}, then self reduction 2 CuX2O+CuX2S→6 Cu+SOX2\ce{2Cu2O + Cu2S -> 6Cu + SO2}. Escaping SOX2\ce{SO2} gives blister copper its look.
  3. 3
    Low grade copper ores are leached with acid or bacteria and CuX2+\ce{Cu^2+} is reduced with scrap iron or HX2\ce{H2}.
  4. 4
    Zinc: ZnO is made into briquettes with coke and clay and reduced by coke at a higher temperature than copper needs; NCERT writes ZnO+C→coke,673 KZn+CO\ce{ZnO + C ->[coke, 673 K] Zn + CO} (other sources put zinc smelting nearer 1300 to 1400 K). The zinc distils off and is collected by rapid chilling.
  • Aluminium (Hall Héroult process): purified AlX2OX3\ce{Al2O3} is mixed with cryolite NaX3AlFX6\ce{Na3AlF6} or CaFX2\ce{CaF2}, which lowers the melting point of the mix (alumina alone melts above 2300 K) and makes it conduct. A steel cell lined with carbon is the cathode; graphite rods are the anodes.
  • Cathode: AlX3++3 eX−→Al(l)\ce{Al^3+ + 3e- -> Al(l)}. Anode: C+OX2−→CO+2 eX−\ce{C + O^2- -> CO + 2e-} and C+2 OX2−→COX2+4 eX−\ce{C + 2O^2- -> CO2 + 4e-}. Overall: 2 AlX2OX3+3 C→4 Al+3 COX2\ce{2Al2O3 + 3C -> 4Al + 3CO2}, so the anodes burn away, about 0.5 kg of carbon per kg of aluminium (NCERT).

Refining

MethodPrincipleMetals
DistillationLow boiling metal is vaporised and condensedZn, Hg
LiquationLow melting metal flows off a sloping hearthSn
ElectrolyticImpure anode, pure cathode, salt solution; less reactive impurities form anode mud (Sb, Se, Te, Ag, Au, Pt)Cu (CuSO₄ + H₂SO₄), Zn
Zone refiningImpurities are more soluble in the melt than in the solid; a moving heater sweeps them to one endSi, Ge, B, Ga, In (semiconductors)
Mond processNi+4 CO→330 to 350 KNi(CO)X4\ce{Ni + 4CO ->[\text{330 to 350 K}] Ni(CO)4}; Ni(CO)X4→450 to 470 KNi+4 CO\ce{Ni(CO)4 ->[\text{450 to 470 K}] Ni + 4CO}Ni
van Arkel methodZr+2 IX2→ZrIX4\ce{Zr + 2I2 -> ZrI4}; ZrIX4\ce{ZrI4} decomposes on a hot W filament (about 1800 K)Zr, Ti
ChromatographyDifferential adsorptionElements in minute amounts

Formula bank

Coupled reduction

ΔGnet∘=ΔG∘(reductant oxidation)−ΔG∘(metal oxidation)<0\Delta G^\circ_{\text{net}} = \Delta G^\circ(\text{reductant oxidation}) - \Delta G^\circ(\text{metal oxidation}) < 0

Faraday’s law

m=M I tnFm = \frac{M\,I\,t}{nF}

Hall Héroult overall

2 AlX2OX3+3 C→4 Al+3 COX2\ce{2Al2O3 + 3C -> 4Al + 3CO2}

Cyanide leaching

4 Au+8 CNX−+2 HX2O+OX2→4 [Au(CN)X2]X−+4 OHX−\ce{4Au + 8CN- + 2H2O + O2 -> 4[Au(CN)2]- + 4OH-}

Self reduction of copper

2 CuX2O+CuX2S→6 Cu+SOX2\ce{2Cu2O + Cu2S -> 6Cu + SO2}

Mond process

Ni+4 CO⇌Ni(CO)X4\ce{Ni + 4CO <=> Ni(CO)4}

Gibbs energy and equilibrium

ΔG∘=−RTln⁡K=−nFE∘\Delta G^\circ = -RT\ln K = -nFE^\circ

Tricks & mnemonics

Calcine carbonates, roast sulfides

“Calcination for Carbonates; Roasting for Rotten egg (sulfide) ores.”

Ellingham rule

Lower line reduces upper line. C→CO is the only common line going down, so carbon wins at high temperature.

Refining matchmaker

Zn/Hg distil, Sn liquates, Cu electrolyses, Si/Ge are zone refined, Ni by Mond, Zr/Ti by van Arkel.

Who does what in Al extraction

Bayer purifies the ore; Hall Héroult electrolyses it; cryolite lowers the melting point and boosts conductivity.

NaCN does two jobs

Depressant for ZnS in froth flotation; complexing agent for Ag/Au in leaching.

NCERT high yield lines

Original NCERT aligned summaries of the lines examiners love. Tap “Quiz me” to test yourself instantly.

  • In froth flotation, collectors such as pine oils, fatty acids and xanthates make the mineral particles less wettable by water, and froth stabilisers such as cresols and aniline stabilise the froth.Class 12 · Isolation of Elements (earlier edition)
  • The Ellingham diagram plots ΔfG° of oxide formation against temperature; the C→CO line slopes downward because the reaction increases the number of gas molecules.Class 12 · Isolation of Elements (earlier edition)
  • In the electrolytic reduction of alumina, cryolite and fluorspar are added to lower the melting point of the mixture and increase its conductivity.Class 12 · Isolation of Elements (earlier edition)
  • In the extraction of copper, Cu₂S and Cu₂O react together in the converter to give copper metal (self reduction); the solidified copper has a blistered appearance due to escaping SO₂.Class 12 · Isolation of Elements (earlier edition)
  • Zone refining is based on the principle that impurities are more soluble in the melt than in the solid state of the metal.Class 12 · Isolation of Elements (earlier edition)

Exceptions to remember

  • Iron pyrites (FeSX2\ce{FeS2}) is not used as an ore of iron.

    NCERT: the abundant oxide ores are preferred because they do not produce polluting gases such as the SO₂ released from pyrites.

  • The 2 C+OX2→2 CO\ce{2C + O2 -> 2CO} line has a negative slope in the Ellingham diagram.

    Gas moles increase, so ΔS is positive.

  • Below about 983 K CO is a better reductant than C; above it carbon is better.

    Crossing point of the CO→CO₂ and C→CO lines.

  • Aluminium is not extracted by carbon reduction.

    Al₂O₃ is extremely stable and carbon would form Al₄C₃ at the required temperature.

  • Copper needs no separate reducing agent in the converter.

    Self reduction: Cu₂S reduces Cu₂O.

  • Silver and gold are extracted by first oxidising them (with OX2\ce{O2}/CN⁻) and then reducing with Zn.

    Hydrometallurgy: soluble cyano complexes form only after oxidation.

  • In zone refining the impurities travel with the molten zone.

    They are more soluble in the melt than in the solid.

  • The graphite anodes are consumed in the Hall Héroult cell.

    Oxide ions discharge as O₂, which burns the carbon to CO and CO₂.

Solved problems

Example 1
JEE MainFoundation
How many faradays are needed to produce 54 g of aluminium in the Hall Héroult cell?
Example 2
JEE AdvancedExam level
At a temperature T (given data): ΔG∘(2 Zn+OX2→2 ZnO)=−360\Delta G^\circ(\ce{2Zn + O2 -> 2ZnO}) = -360 kJ and ΔG∘(2 C+OX2→2 CO)=−460\Delta G^\circ(\ce{2C + O2 -> 2CO}) = -460 kJ. Is the reduction of ZnO by carbon feasible at T?
Example 3
JEE MainJEE AdvancedFoundation
Explain the roles of NaCN and of zinc in the extraction of silver.
Example 4
JEE MainExam level
A current of 9.65 A is passed through molten alumina for 10 000 s. What mass of aluminium is deposited?

Practice

Q1
Matrix match
JEE AdvancedExam level
Important
Match the reagent with its role.
Column I: (P) cryolite in aluminium extraction (Q) NaCN in froth flotation of PbS and ZnS (R) silica in copper smelting (S) zinc in the cyanide process
Column II: (1) reducing agent (2) depressant (3) flux that removes iron oxide as slag (4) lowers the melting point and raises conductivity
Q2
Matrix match
JEE AdvancedFoundation
Important
Match the refining method with the metal.
Column I: (P) distillation (Q) liquation (R) van Arkel (S) Mond
Column II: (1) Ni (2) Sn (3) Zr (4) Zn
Q3
Single correct
JEE AdvancedExam level
Important
In the Ellingham diagram, the line with a negative slope is:
Q4
One or more correct
JEE AdvancedAdvanced
Important
Which statements about the Ellingham diagram are correct?
Q5
Single correct
JEE AdvancedFoundation
Important
In froth flotation of an ore containing both PbS and ZnS, the depressant used is:
Q6
Single correct
NEETFoundation
Bauxite is an ore of:
Q7
Single correct
NEETFoundation
Calcination is used mainly for:
Q8
Numerical
JEE MainFoundation
Number of faradays required to produce 54 g of Al from AlX3+\ce{Al^3+}:
Q9
One or more correct
NEETJEE MainFoundation
Which are purified by zone refining?
Q10
Single correct
NEETFoundation
The Mond process is used to refine:
Q11
Single correct
NEETFoundation
Cryolite is added in the electrolytic extraction of Al to:
Q12
Single correct
NEETJEE MainFoundation
In the cyanide process, gold is recovered from [Au(CN)X2]X−\ce{[Au(CN)2]-} by adding:
Q13
Numerical
JEE MainJEE AdvancedExam level
Mass of Al (g) deposited by 9.65 A passed for 10 000 s:
Q14
Single correct
NEETFoundation
Blister copper gets its appearance from:
Q15
Single correct
JEE AdvancedExam level
Most lines in the Ellingham diagram for the formation of metal oxides slope upward because:
Q16
Single correct
JEE AdvancedExam level
Which reaction takes place in the cooler upper zone (500 to 800 K) of the blast furnace?
Q17
One or more correct
JEE MainJEE AdvancedExam level
Which statements about the Hall Héroult process are correct?
Q18
Single correct
JEE AdvancedExam level
Which pair of ores is usually concentrated by froth flotation?
Q19
Single correct
JEE AdvancedExam level
In the converter, 2 CuX2O+CuX2S→6 Cu+SOX2\ce{2Cu2O + Cu2S -> 6Cu + SO2}. Which species acts as the reducing agent?
Q20
Numerical
JEE AdvancedExam level
What mass of NaOH (in kg) is needed to dissolve 1020 kg of pure AlX2OX3\ce{Al2O3} in the Bayer process, AlX2OX3+2 NaOH+3 HX2O→2 Na[Al(OH)X4]\ce{Al2O3 + 2NaOH + 3H2O -> 2Na[Al(OH)4]}? (Al = 27, O = 16, Na = 23, H = 1)
Q21
Single correct
JEE AdvancedExam level
Impure copper containing Zn, Fe, Ag and Au is refined electrolytically. Which impurities collect in the anode mud?
Q22
Numerical
JEE AdvancedAdvanced
An aluminium cell runs at 100 kA for 24 h with 90% current efficiency. What mass of aluminium (in kg) is produced? (F = 96500 C mol⁻¹, Al = 27)
Q23
Numerical
JEE AdvancedAdvanced
Take ΔG∘\Delta G^\circ for 2 Fe(s)+OX2(g)→2 FeO(s)\ce{2Fe(s) + O2(g) -> 2FeO(s)} as (−540+0.140T)(-540 + 0.140T) kJ and for 2 C(s)+OX2(g)→2 CO(g)\ce{2C(s) + O2(g) -> 2CO(g)} as (−220−0.158T)(-220 - 0.158T) kJ, with T in kelvin. Above what temperature (in K, nearest integer) can coke reduce FeO to iron?
Q24
Numerical
JEE AdvancedAdvanced
Pig iron containing 4.0% carbon is converted to wrought iron in a furnace lined with haematite, which oxidises the carbon: FeX2OX3+3 C→2 Fe+3 CO\ce{Fe2O3 + 3C -> 2Fe + 3CO}. What mass of FeX2OX3\ce{Fe2O3} (in kg) is needed to remove all the carbon from 1000 kg of pig iron? (Fe = 56, C = 12, O = 16)
Q25
Numerical
JEE AdvancedAdvanced
In the converter, part of the CuX2S\ce{Cu2S} is oxidised (2 CuX2S+3 OX2→2 CuX2O+2 SOX2\ce{2Cu2S + 3O2 -> 2Cu2O + 2SO2}) and the oxide then reacts with more sulfide (2 CuX2O+CuX2S→6 Cu+SOX2\ce{2Cu2O + Cu2S -> 6Cu + SO2}). What volume of SOX2\ce{SO2} (in L at STP, molar volume 22.4 L) is released per 127 g of copper produced? (Cu = 63.5)

Ready for the real thing?

Take a timed, NTA style test on this chapter with instant analytics